Concrete cracks. What matters is where.

Cracks in concrete form inevitably through shrinkage, temperature changes and loading. They are a physical phenomenon, not a construction defect. What matters is not preventing cracks, but controlling them: through targeted crack induction using crack inducers in new builds, or through crack and joint injection with acrylate and polyurethane resins in existing structures. The governing standard for crack width limitation is SIA 262 in Switzerland and DIN EN 1992-1-1 (Eurocode 2) in Germany.

One of the most persistent misconceptions in construction is that cracks in concrete are a sign of poor workmanship. In reality, they are unavoidable. The key question is not “How do I prevent cracks?” but “How do I deal with them correctly?” — and this is precisely where good structural waterproofing is separated from excellent structural waterproofing.

Why Does Concrete Crack?

Concrete is a living material. It shrinks as it cures, expands and contracts with temperature fluctuations, and deforms under load. Added to this are restraint stresses — for example when a freshly cast element is connected to an older one. The formation of microcracks in this process is normal; it is the way concrete relieves stress.

 

Cracks only become a problem when they propagate uncontrolled, allow water ingress or endanger the reinforcement. This risk is amplified in today’s construction practice: concrete is often cured rapidly and loaded early, leading to more and larger cracks. Calling for “more steel” does not address the root cause. Often the real issue lies in inadequate or poor curing — fresh concrete that is not kept sufficiently moist and protected from drying out too quickly.

Two Classic Approaches — and Their Limitations

Conventionally, cracks are either prevented through heavy reinforcement or controlled using mechanical means such as waterstops. Both have their place, but also their weaknesses. More steel means higher costs, greater weight and a worse CO₂ footprint. Mechanical waterstops rely on careful installation and offer little room for manoeuvre when retrospective action is needed. 

 

RASCOR has pursued a third approach for decades: directing cracks deliberately to locations where they can occur in a controlled manner – and sealing them reliably at those points. Instead of fighting cracks, you plan for them.

 

Controlled Crack Management with the Crack Inducer
At the heart of this approach is the RASCOtec Crack Inducer. Installed within the concrete, it deliberately weakens the element at a defined location. When tensile stress occurs, the concrete does not crack randomly — it cracks where the crack inducer is positioned. An injection channel is placed directly alongside it, protecting the resulting crack from water ingress.

Comparison: Crack Prevention versus Crack Control

CriterionCrack prevention (more reinforcement)Crack control (crack inducer)
Basic principleDistribute and minimise cracks using steelDirect cracks to planned locations
Reinforcement requirementHighReduced
Concreting sectionsLimited by shrinkage reinforcementLarge sections possible
Location of cracksRandom within the elementPredefined and protected
Retrospective treatmentComplex — crack must be locatedDirectly accessible via injection channel
CO₂ footprintWorse due to higher steel consumptionBetter due to material savings

When the Crack Is Already There: Injection as a Remediation Method

Not every crack forms where it is expected. In existing structures, or where no crack inducer was provided, cracks can appear unplanned – and still need to be permanently sealed. In many cases, cracks have already formed, water is entering and reinforcement is beginning to corrode. For all these situations, RASCOR offers a coordinated portfolio of two main families of injection resins.

  • Polyurethane resins react with water and foam up. Ideal for actively water-bearing cracks, as they cure reliably even in the presence of moisture.

  • Acrylate gels are low-viscosity and elastic, penetrating deep into the finest crack systems. Perfect for branching damage patterns and joint injections.

Application is carried out via bore holes and packers – precise, with minimal structural intervention and minimal downtime. Particularly in structures in continuous operation, such as underground car parks, this is a decisive advantage.

What Planners Should Consider Early On

Most damage can be avoided when the waterproofing concept is addressed at the start of the planning process. Three questions usually go a long way:

  • Where will the concrete crack? Structural engineers and waterproofing specialists should jointly identify the areas where tensile stresses will develop.

  • Where can I make adjustments later? Providing injection channels is inexpensive at the planning stage — and costly if they are missing.

  • What loads will actually occur? Hydrostatic pressure, chemical exposure, movement — every requirement calls for the right material system.
Frequently asked questions
Are cracks in concrete a construction defect?

No. Cracks form inevitably in all concrete through shrinkage, temperature and loading. A construction defect only exists when crack widths exceed the normative limits, or when cracks lead to water ingress and reinforcement corrosion.

The permissible crack width depends on the intended use and exposure class. It is governed by SIA 262 and Eurocode 2 respectively and typically ranges from 0.1 to 0.4 millimetres depending on requirements. Stricter values apply for watertight structures.

Injection resins are introduced into the crack via bore holes and packers. Polyurethane resins are suitable for water-bearing cracks; acrylate gels for fine, branching crack systems. The resin reacts within the crack and seals it permanently.

A crack inducer is a profile installed within the concrete that deliberately weakens the element at a defined point. This causes the crack to form at a planned location rather than randomly. An injection channel positioned directly alongside protects the crack from water ingress.

This depends on water flow, crack width, element movement and substrate. Water-bearing cracks require reactive polyurethane resins; dry or fine cracks are better suited to acrylate gels. An informed choice requires an assessment of the damage pattern.

Conclusion:

Cracks in concrete are neither poor workmanship nor a mistake — they are physics. Those who treat them as the enemy are fighting a losing battle. Those who understand and plan for them build structures that remain watertight for a lifetime. This is the essence of preventive waterproofing — and for 60 years, it is what has distinguished RASCOR materials.

.

Are you planning a project involving controlled crack management or do you need the right injection system?

Contact us for targeted product advice on our proven waterproofing materials. Contact: +41 44 857 11 11 or sales@rascor.com.

 

Leave a comment

Your email address will not be published. Required fields are marked *